Finding · as stated by the study, recorded by Coridum · status verified-machine
Finding F-0326
“In second place, pine showed relatively high emissions (0.0127 ± 0.002 μg g−1 ), followed by birch (0.0109 ± 0.001 μg g−1 ) and MDF (0.0107 ± 0.0002 μg g−1 ), whose values were statistically close within the margin of experimental error.”
Structure
- Source
- Wood
- Factor
- Formaldehyde (CH₂O)
- Setting
- laboratory (desiccator), MX
- Study design
- laboratory desiccator-method comparison (JIS A 1460 type) of formaldehyde emissions from six interior wood materials: medium-density fiberboard, melamine-faced board, pine, birch, oak and alder (class 4)
- Effect
- emission-rate 0.0127
- Caveat
- emission per gram of material in a desiccator, not a room concentration; spread printed as ± without naming the measure
A Finding records what one published document states, verbatim and with its page. It is not a conclusion of Coridum; see the Claims that build on it.