“On the other hand, oak (0.0063 ± 0.0002 μg g−1 ) and alder (0.0023 ± 0.0001 μg g−1 ) showed the lowest emissions, demonstrating a lower potential contribution to the release of HCHO in indoor environments.”
Structure
- Source
- Wood
- Factor
- Formaldehyde (CH₂O)
- Setting
- laboratory (desiccator), MX
- Study design
- laboratory desiccator-method comparison (JIS A 1460 type) of formaldehyde emissions from six interior wood materials: medium-density fiberboard, melamine-faced board, pine, birch, oak and alder (class 4)
- Effect
- emission-rate 0.0023
- Caveat
- emission per gram of material in a desiccator, not a room concentration; spread printed as ± without naming the measure